Vigorously develop circular economy: the company adheres to the development path of circular economy, realizes the efficient utilization of energy and EN 10025 S420ML steel plate resources, implements "four closed circuits" for renewable gas, industrial water, solid waste and waste heat steam according to the reduction of resource consumption - reuse - recycling, vigorously promotes advanced technologies such as energy-saving new technologies, new processes, EN 10025 S420ML steel plate new materials, and promotes the competition of enterprises Struggle.
How to prevent EN 10025 S420ML steel plate, steel plate cutting cracks? 1. Preheat the steel plate before cutting, and the preheating temperature depends on the quality grade and thickness of the steel plate. However, it needs to be heated evenly. 2. The cutting speed is reduced appropriately, but its reliability is not as good as preheating. It is suggested to preheat the cutting belt with flame gun cavitation several times before cutting, and the preheating temperature should reach about 180℃.
In actual processing applications, the processing EN 10025 S420ML steel plate thickness of flame cutting ranges from 6 to 200 mm, and the EN 10025 S420ML steel plate cutting thickness can even reach 350 mm by replacing the air pipe and cutting torch nozzle. In order to better improve the cutting quality, the related process parameters will be slightly different when using flame cutting for materials of different thickness. The verticality of the cutting surface processed by the CNC flame cutting machine is generally high, and the slope can be controlled below 2-3°. The characteristic is that flame cutting performs better when cutting EN 10025 S420ML steel plate with a certain thickness above 10mm.
A514 Gr A structural steel plates are mainly used in cranes or large heavy-load machines. ASTM A514 steel offers high strength with weldable, machinable properties.Quenched and tempered for increased strength.Available in eight grades: B, S, H, Q, E, F, A and P.Available in heavy plate thicknesses (3-inches or greater).Suitable in lower temperatures. Charpy impact test results for specific climates available.