How to distinguish the inferior steel plate? 1. The surface of the fake and inferior steel plate is easy to produce scab. 2. The material of fake and inferior steel plate is not uniform and there are many impurities. The surface of fake and inferior steel plate is often pitted. Pitting is an irregular and uneven defect on the surface of S275M steel supplier, steel plate caused by serious wear of rolling groove. Due to the pursuit of profit by the manufacturers of fake and inferior steel plates, the groove rolling often exceeds the standard.

A514 gr.H quenched and tempered alloy steel sheet chemical composition (melting analysis)%C: 0.12-0.21, Si: 0.20-0.35, Mn: 0.95-1.30, P max.: 0.035, S max.: 0.035, Cr: 0.40-0.65, Ni: 0.30-0.70, Mo: 0.20-0.30, V: 0.03-0.08, B: 0.001-0.005The mechanical properties in thickness (mm)T≤65Yield strength (≥Mpa): 690Tensile strength (Mpa):760-895Elongation in ≥, %: 18

Rizhao Steel 5#ESP Headless Strip Production Line Project is a key construction project in Shandong Province. It is also the fifth domestic ESP production line introduced by Rizhao Steel and the sixth ESP production line in the world. Its thinnest design is 0.5mm, which is at the world's leading level. The more than 20 important nodes set by the entire project have been basically completed, and the equipment has entered the commissioning stage. It is expected to be put into operation at the end of November.

Previous:Some details of EN 10025 S275M steel pla Next:Steel Industry S355ML material propertie

Add Your Comments

First Name*

Tel*

Email*

Your Comments*